Rated on 5 criteria: print temperature, warping, strength, creep resistance, and heat resistance (★1-5).
Nozzle: 210-230°C
Bed: 40-60°C
Flexible
Not measured
Different rating for flexible material
Heat Resistance Temp: 70°C
| Item | Recommended Value | Notes |
|---|---|---|
| Nozzle Temperature | 210-230°C | Adjust by hardness |
| Bed Temperature | 40-60°C | Improves adhesion |
| Fan Setting | 50-100% | Overhangs only |
| Print Speed | 15-30mm/s | Slow speed required |
| Nozzle Diameter | 0.4-0.6mm | Larger diameter more stable |
| Retraction | 1-3mm | Minimize |
| Caution | Direct drive recommended, slow speed | |
| Item | Measured Value |
|---|---|
| Default (Flat Layout) | |
| Bending Strength | N/A |
| Flexural Modulus | N/A |
| Test Method | 3-Point Bending Test(Details) |
Bending test data for this filament has not been registered yet.
The graph will be displayed once data is added.
TPU has various variations based on hardness.
Standard hardness. Balanced flexibility and printability.
Slightly harder. Easier to print with good mechanical strength.
Very flexible. Rubber-like texture, high print difficulty.
Carbon fiber reinforced. Maintains flexibility with improved strength.
• Direct drive extruder printing is strongly recommended.
• Set print speed to slow 15-30mm/s.
• Minimize retraction settings to prevent stringing.