Rated on 5 criteria: print temperature, warping, strength, creep resistance, and heat resistance (★1-5).
Nozzle: 260-310°C
Bed: 90-110°C
Prone to warping
Bending Strength: (110.00 MPa)
Rated
Heat Resistance Temp: 130°C
| Item | Recommended Value | Notes |
|---|---|---|
| Nozzle Temperature | 270-310°C | High-temp nozzle required |
| Bed Temperature | 110-130°C | High-temp bed required |
| Fan Setting | 0% | No cooling |
| Print Speed | 20-40mm/s | Slow for stability |
| Nozzle Diameter | 0.4-0.6mm | Hardened steel |
| Chamber Temp | 60-80°C | Enclosed chamber required |
| Caution | Drying required, high-temp equipment needed | |
| Item | Measured Value |
|---|---|
| Default (Flat Layout) | |
| Bending Strength | 110 MPa |
| Flexural Modulus | N/A |
| Test Method | 3-Point Bending Test(Details) |
Bending test data for this filament has not been registered yet.
The graph will be displayed once data is added.
Various derivative filaments with enhanced properties have been developed based on PC.
Standard PC. Extremely high heat resistance and strength, industrial-grade performance.
Carbon fiber reinforced. Aerospace-grade performance, extremely expensive.
Glass fiber reinforced. Maximum dimensional stability and strength.
• Very high print temperature (270-310°C); limited compatible printers.
• Highly hygroscopic; drying required.
• Enclosed chamber printing strongly recommended.
• Advanced material.